您好!欢迎您访问无锡市云坤钢管有限公司网站!
35crmo淬火后硬度@无锡35crmo气瓶无缝管淬火工艺
屈服强度 σs (MPa):≥835(85)
伸长率 δ5 (%):≥12
冲击韧性值 αkv (J/cm2):≥78(8)
硬度 :≤229HB
无缝管现货规格
25×6 |
28×6 |
32×6-8 |
34×6-8 |
36×6-8 |
38×6-7-8-9-10 |
39×8-10 |
42×6-7-8-9-10 |
45×6-7-8-9 |
48×6-7-8-9-10 |
51×6-7-8-9-10 |
56×6-7-8-9-10 |
57×6-7-8-9-10-12 |
60×6-7-8-9-12-14 |
63×6-7-8-9-10-12-14 |
68×6-7-8-9-10-12-14-16 |
70×6-7-8-9-10-12-15-16 |
73×6-7-8-9-10-12-15 |
76×6-7-8-9-10-12-14 |
|